中文摘要: 针对高碳铅锌银多金属硫化矿难选的问题,对某高碳硫化矿进行了试验研究。该矿中铅品位3.72%,锌品位8.34%,银品位34.13g/t。通过流程探索,确定了预先脱碳-铅锌优先浮选工艺流程。在此基础上进行了条件试验研究,确定适宜磨矿细度为-0.074mm占90%。确定最佳药剂制度为:铅浮选ZnSO4 Na2SO3用量为2000g/t,组合捕收剂乙硫氮和丁铵黑药用量为80g/t 50g/t,锌浮选硫酸铜用量为800g/t,丁基黄药用量为100g/t。经闭路流程试验,得到最终指标为:铅精矿中Pb品位52.14%,回收率为88.54%,伴生银的品位为368.50g/t,回收率68.04%,锌精矿品位60.23%,回收率为90.16%。
Abstract:In view of the high carbon polymetallic sulphide ore of lead zinc and silver is difficult to flotation; the large experiment study was done. The grade of Lead is 3.72%, the grade of Zinc is 8.34%, and the silver grade is 34.13g/t. Through the process exploration experiment, the decarbonization and selective flotation flowsheet of Pb-Zn was determined. The appropriate grinding fineness is -0.074mm 90% by the condition test experiment. The reagent systems of Lead were the ZnSO4 Na2SO3 dosage 2000g/t, the combined collector of ethyl thio carbamate and ammonium butyl aerofloat (80, 50) g/t. The reagent systems of Zinc were the copper sulfate dosage 800g/t, the butyl xanthate dosage 100g/t. Through the closed circuit process, the grade of Pb is 52.14% and the recovery is 88.54%, the associated silver grade is 368.50g/t and the recovery is 68.04% in the Lead concentrate. The grade of Zn is 60.23% and the recovery is 90.16% in the Zinc concentrate.
keywords: High carbon Lead zinc sulfide minerals Flotation Silver
文章编号:20141216001 中图分类号: 文献标志码:
基金项目:
引用文本:
杨俊龙,孙运礼,郭艳华.某高碳铅锌银多金属硫化矿浮选试验研究[J].矿冶,2016,25(1):26~30.
杨俊龙,孙运礼,郭艳华.某高碳铅锌银多金属硫化矿浮选试验研究[J].矿冶,2016,25(1):26~30.