复杂多金属尾矿伴生金银铁综合回收试验研究
周光浪, 周东云
(云南黄金矿业集团股份有限公司)
Experimental study on comprehensive recovery of gold, silver and iron associated with complex polymetallic tailings
ZHOU Guang-lang, ZHOU Dong-yun
(Yunnan Gold Mining Group Co. Ltd.)
摘要
图/表
参考文献
相似文献
本文已被:浏览 552次   下载 364
投稿时间:2022-04-07    修订日期:2022-04-12
中文摘要: 为综合回收某复杂多金属浮选尾矿中伴生的金银铁,分别开展了磁选、全泥氰化浸出、反浮选试验研究。结果表明,优先采用强磁预选抛尾的方法对含铁矿物进行富集,再采用先回收金银后选铁的方案较好。矿石在“强磁抛尾-全泥氰化浸出-弱磁选铁-强磁选铁,磁铁精矿反浮选脱硫”的联合工艺下,金、银浸出率分别达85.32%和72.13%,并获得TFe品位为62.01%,TFe回收率为11.04%,含硫量为0.25%磁铁精矿,及TFe品位为45.30%,TFe回收率为18.54%铁精矿产品。
中文关键词: 磁选  全泥氰化浸出  反浮选脱硫
Abstract:In order to comprehensively recover the gold, silver and iron associated with a complex polymetallic flotation tailings, magnetic separation, full-slime cyanidation leaching and reverse flotation were carried out respectively. The results show that it is better to use the strong magnetic pre-selection tail-throwing method to enrich iron-bearing minerals first, and then use the scheme of recovering gold and silver first and then selecting iron. Under the combined process of "strong magnetic tail throwing-full mud cyanidation leaching-weak magnetic iron separation-strong magnetic iron separation, reverse flotation desulfurization of magnetite concentrate", the leaching rates of gold and silver reached 85.32% and 72.13% respectively. And obtained TFe grade of 62.01%, TFe recovery rate of 11.04%, magnetite concentrate with sulfur content of 0.25%, and TFe grade of 45.30%, TFe recovery rate of 18.54% iron concentrate products.
文章编号:20220407001     中图分类号:    文献标志码:
基金项目:
引用文本:
周光浪,周东云.复杂多金属尾矿伴生金银铁综合回收试验研究[J].矿冶,2022,31(5):.

为了给您提供更优质的网页浏览体验,请使用 Firefox 、Chrome、IE10、IE11、360极速模式、搜狗极速模式、QQ极速模式等浏览器,其他浏览器不建议使用

我们一直在努力打
造,精品期刊,传
播学术成果

全国咨询服务热线
010-63299751

杂志信息

期刊简介

相关下载

联系我们

电话:010-63299751

传真:010-63299754

QQ:XXXXXXX

Email:kuangye@bgrimm.com

邮编:100160

地址:北京市南四环西路188号总部基地十八区23号楼905 北京矿冶研究总院《矿冶》编辑部

关注微信公众号