中文摘要: 河南某钼矿尾矿中钼主要以辉钼矿形式赋存,辉钼矿分布在-530+125μm和-38μm的粒级中,脉石矿物主要为钙铁石榴石及石英,该实验采用HydroFloat水力浮选机对粗颗粒钼尾矿进行分选,达到抛尾的目的。HydroFloat水力浮选机采用流化床技术对矿物进行浮选,同时在选别过程中引入上升水流,使粗颗粒能够克服重力随气泡上升从而达到富集的目的。经水力浮选抛尾后,可将原矿中品位为0.033%的钼富集得到品位为0.081%,回收率为92.18%钼粗精矿,抛尾率为66.91%。
Abstract:The molybdenum in the tailings of a molybdenum mine in Henan is mainly in the form of pyromorphite, distributed in the -530+125μm and -38μm grain sizes, and the vein minerals are mainly calcite-garnet and quartz. Flotation is achieved by introducing an upward flow of water during the separation process, allowing the coarse particles to overcome gravity and rise with the air bubbles. The hydro flotation tailings enrich 0.033% of the molybdenum in the original ore to produce a crude molybdenum concentrate with a grade of 0.081% and a recovery of 92.18%, giving a tailings recovery of 66.91%.
文章编号:20230411002 中图分类号: 文献标志码:
基金项目:国家自然科学基金项目(面上项目,重点项目,重大项目)
引用文本:
熊宇农,封东霞,童雄,李容娇,罗亨通,张小永.粗颗粒钼尾矿水力浮选试验研究[J].矿冶,2023,32(5):.
熊宇农,封东霞,童雄,李容娇,罗亨通,张小永.粗颗粒钼尾矿水力浮选试验研究[J].矿冶,2023,32(5):.