| THE STUDY ON RECOVER LOW GRADE FLUORITE IN POLYMETALLIC ORE TAILINGS |
|
Received:February 26, 2013
Revised:February 28, 2013
Accepted:March 07, 2013
Published Online:August 23, 2013
|
| View Full Text View/Add Comment Download reader |
| DOI: |
| KeyWord:polymetallic ore tailing; low grade fluorite; flotation |
| Author | Institution |
| SUN Zhijian |
Beijing General Research Institute of Mining and Metallurgy |
|
| Hits: 2792 |
| Download times: 17 |
| Abstract: |
| The grade of CaF2 in a polymetallic ore tailing in YunNan is 6.51%. After hydrocyclone desliming, iron removal by magnetic separation, sulphide mineral removal by flotation, six times cleaning using acidic sodium silicate and sodium hexametaphosphate, impurity removal by high-intensity magnetic separation, the fluorite concentrate containing CaF2 95.68% can be obtained. |
| Close |
|
|
|