| Preparation of Sodim Jarosite fromNickel Laterite |
|
Received:August 16, 2017
Revised:March 23, 2018
Accepted:September 06, 2017
Published Online:May 25, 2018
|
| View Full Text View/Add Comment Download reader |
| DOI: |
| KeyWord:laterite-nickel ore; sodium jarosite; comprehensive utilization |
| Author | Institution |
| CHANG Long-jiao |
College of New Energy,Bohai University |
| LIU Jia-nan |
College of New Energy,Bohai University |
| LIU Lian-li |
College of New Energy,Bohai University |
| ZHAI Yu-chun |
College of Materials and Metallurgy,Northeastern University |
| WU Yan |
College of Materials and Metallurgy,Northeastern University |
|
| Hits: 1955 |
| Download times: 1404 |
| Abstract: |
| To obtain the appropriate conditions for eliminating Fe3 from NiSO4 solution, the digestion solution of the clinker was used as raw material, which was obtained from roasting the nickel oxide ore with (NH4)2SO4. and Na2CO3 as alkaline regulator, the wet chemisty method was prepared the ammonium jarosite(Na2Fe6(SO4)(OH)12). The optimum technological conditions are reaction temperature at 95℃, reaction time at 4h, the end pH level at 2.5, the iron removal rate over 99.5% under the optimum conditions. The XRD、SEM and componebts analysis were used to characterize the decomposition product. The Na2Fe6(SO4)(OH)12 with regular cluster figure is composed of sheet particles with smooth surface. |